CHEMISTRY
Silicon | 0.2 – 0.8% |
Manganese | 0.4 – 0.9% |
Chromium | 16 – 16.7% |
Nickel | 4 – 4.5% |
Phosphorus | 0.04% max |
Molybdenums | 0.15 – 0.35% |
Copper | 3.90 – 4.50% |
Niobium | 0.2 – 0.4% |
Oxygen | 0.08% max |
Nitrogen | 0.09% max |
Carbon | 0.05% max |
Sulfur | 0.03% max |
PROPERTIES
Shape | Spherical |
Density | 7.7 – 7.8 g/cc |
Tap Density | 4.7 g/cc min |
Hall Flow | 15 seconds max* |
Carney Flow | 5 seconds max* |
* For part numbers beginning R0106
ORDER INFORMATION
Part Number | Particle Size min | Particle Size max | Price per kg |
R0106-N-00-2003 | 44 microns | 106 microns | $36.00 |
R0028-N-00-0003 | 0 microns | 28 microns | $46.00 |
Packaging available in 12.5 kg plastic pails
and 225 kg fiber drums
To order, email customer service at:
cs@ervinindustries.com
Stainless steel metal powder is commonly used in
3-D printing.
Thermal spray and cold spray are two technologies that utilize stainless steel metal powders in numerous coating applications.
In the aerospace, medical, and automotive industries, processes like hot isostatic pressing
(HIP) utilize stainless steel metal powders to produce precise, high-integrity components and parts.